Spectral resolved absorption/transmittance measurement

CIMPS-ABS

CIMPS-ABS including spectrometer with measurement and reference cells
Light absorption spectra vs applied voltages measured by CIMPS-ABS
CIMPS-ABS allows spectral resolved transmittance / absorbance measurements to characterize electro-chromic processes. It can be used with an LED-emitter or tungsten lamp. The transmittance / absorbance spectrum can be measured for different bias voltages or currents, time, or any other control parameter like temperature, pH, or concentration etc.

In CIMPS-ABS, two PECC-2 cells are mounted and used sequentially. One PECC-2 cell is used as a reference whereas the other is used for measurement. The reference cell aids in mitigating the artefacts due to light loss via reflection or electrolyte absorption which in turn helps in accurately measuring the absorption spectrum.
  • ABS-1: Beam diameter      = 18 mm
  • ABS-1: Wavelength range = 420 - 730 nm
  • ABS-2: Beam diameter      = 600 µm
  • ABS-2: Wavelength range = 215 - 1100 nm

Specifications

Spectrometer ILT960
Intensity calibrated spectroradiometer



Integration time: 1 ms - 60 s
Accuracy:

350 - 450 nm: ±10%

450 - 900 nm: ±5%

900 - 1050 nm: ±10%
Accessories
2 x PECC-2
Light source
LSW-1 LED (420 - 730 nm)
Software
CIMPS-abs software
Spectrometer
Ultra low straylight fiber optic spectrometer
Light source
balanced tungsten-deuterium light source (215–1100 nm)
Software
CIMPS abs software
Accessories
2 x PECC-2 Q
Spectrometer ILT960
Intensity calibrated spectroradiometer



Integration time: 1 ms - 60 s
Accuracy:

350 - 450 nm: ±10%

450 - 900 nm: ±5%

900 - 1050 nm: ±10%
Accessories
2 x PECC-2
Light source
LSW-1 LED (420 - 730 nm)
Software
CIMPS-abs software
Spectrometer
Ultra low straylight fiber optic spectrometer
Light source
balanced tungsten-deuterium light source (215–1100 nm)
Software
CIMPS abs software
Accessories
2 x PECC-2 Q

Downloads

Download the latest manual add-on about ZAHNER CIMPS system...

Download the latest manual about ZAHNER CIMPS-abs system...

Request a quote

Is this the right product for you? Contact our sales team to get further information about our products and their suitability to your individual applications.

Contact Sales