Power potentiostat

PP212

PP212 Potentiostat with 10 A current range for fuel cell & electrolyzer research
Back panel of the PP212 potentiostat with ethernet and mains connection
Zahner's IM7 potentiostat with PP212 extension for 10 A current range
Accuracy contour plot of Zahner PP212 potentiostat
The PP212 is a 4-quadrant power potentiostat designed to apply and sink high currents up to ±10 A at a high voltage range of up to ±20 V (max. power output 200 W).

For medium power applications, the PP212 is used as an extension of the IM7/ZENNIUM series potentiostat. Most electrochemical techniques which can be performed with the main IM7/ZENNIUM potentiostat can also be carried out with the extended power potentiostat PP212 setup.

Besides an extension, the PP212 power potentiostat can also be used in standalone mode for standard DC measurements i.e., charging/discharging of batteries.

The Zahner's power potentiostats can be incorporated in a Python lab environment and can be used as standalone or in multi-channel configurations. A GitHub repository with examples is available for developing Python applications.
  • Power extension of IM7/ZENNIUM potentiostat for battery, fuel cells, or electrolyzer stack measurements
  • Standalone operation
  • Possible integration in a Python work environment
Potentiostatic modes
potentiostatic, galvanostatic, OCP
Cell connection
2-, 3-, 4-terminal sensing
Ground reference
grounded, floating
Compliance Voltage
±20 V
Maximum current
±10 A
Output power
200 W
Power dissipation
250 W
Input impedance
2 MΩ
Equivalent input noise
< 10 µV rms
Memory
64 GB
Interface
USB, Ethernet (2)
Additional I/Os
5 (2)
Additional analog outputs
1 (2)
Additional analog inputs
4 (2)
Temperature sensor interface
Type K (2)
Ambient temperature
10 °C - 30 °C
Maximum humidity
60 %
Dimensions (H x W x D)
160 x 364 x 378 mm3
Weight
10.2 kg
(2)Hardware features will be unlocked in future with a free software update
Maximum voltage accuracy
±500 µV ±0.1% of reading
Maximum current accuracy
±400 µA ​±0.2% of reading
ADC resolution
24 bits
Input voltage resolution
1.192 µV
Input current resolution
5.96 nA
DAC resolution
16 bits
Output voltage resolution
250 µV
Output current resolution
12.5 µA
Frequency range
10 µHz - 200 kHz (Thales XT)
10 µHz - 400 kHz (Zahner Lab)
Impedance range
1 µΩ - 1 kΩ(1)
(1)Impedances below 1 mΩ must be measured galvanostatically
Maximum voltage accuracy
±500 µV ±0.1% of reading
Maximum current accuracy
±400 µA ​±0.2% of reading
ADC resolution
24 bits
Input voltage resolution
1.192 µV
Input current resolution
5.96 nA
DAC resolution
18 bits
Output voltage resolution
76.3 µV
Output current resolution
3.81 µA
Potentiostatic modes
potentiostatic, galvanostatic, OCP
Cell connection
2-, 3-, 4-terminal sensing
Ground reference
grounded, floating
Compliance Voltage
±20 V
Maximum current
±10 A
Output power
200 W
Power dissipation
250 W
Input impedance
2 MΩ
Equivalent input noise
< 10 µV rms
Memory
64 GB
Interface
USB, Ethernet (2)
Additional I/Os
5 (2)
Additional analog outputs
1 (2)
Additional analog inputs
4 (2)
Temperature sensor interface
Type K (2)
Ambient temperature
10 °C - 30 °C
Maximum humidity
60 %
Dimensions (H x W x D)
160 x 364 x 378 mm3
Weight
10.2 kg
(2)Hardware features will be unlocked in future with a free software update
Maximum voltage accuracy
±500 µV ±0.1% of reading
Maximum current accuracy
±400 µA ​±0.2% of reading
ADC resolution
24 bits
Input voltage resolution
1.192 µV
Input current resolution
5.96 nA
DAC resolution
16 bits
Output voltage resolution
250 µV
Output current resolution
12.5 µA
Frequency range
10 µHz - 200 kHz (Thales XT)
10 µHz - 400 kHz (Zahner Lab)
Impedance range
1 µΩ - 1 kΩ(1)
(1)Impedances below 1 mΩ must be measured galvanostatically
Maximum voltage accuracy
±500 µV ±0.1% of reading
Maximum current accuracy
±400 µA ​±0.2% of reading
ADC resolution
24 bits
Input voltage resolution
1.192 µV
Input current resolution
5.96 nA
DAC resolution
18 bits
Output voltage resolution
76.3 µV
Output current resolution
3.81 µA

Downloads

Access the latest manual about PP2X2 or XPOT2 potentiostat.

Download the latest manual about PP2X2 or XPOT2 potentiostat.

Download 3D Model of PP212 in step file format.

Request a quote

Is this the right product for you? Contact our sales team to get further information about our products and their suitability to your individual applications.

Contact Sales