True IPCE
For incident photons to current efficiency (IPCE) measurements, the CIMPS system can be equipped with the CIMPS-PCS extension, including a tunable light source (TLS). The TLS makes use of an active feedback loop to ensure accurate light illumination. Equipped with up to 29 LEDs and a monochromator, the TLS provides a wavelength resolution down to 1 nm in the visible light range.
The system measures the IPCE using sine-wave modulation of the light source, allowing for the measurement of true IPCE.
The CIMPS system, extended with CIMPS-PCS, can also be used for standard electrochemical and photoelectrochemical techniques which are possible with the CIMPS system.
Methods
- Incident photon to current efficiency (IPCE)
- Chopped light voltammetry (CLV)
- Controlled intensity modulated photocurrent spectroscopy (controlled IMPS)
- Controlled intensity modulated photovoltage spectroscopy (controlled IMVS)
- Maximum power and fill factor measurements
- Light transient measurements
- Time domain measurements
- Standard electrochemical measurements
Technical Specifications
IPCE System
| Parameter | Value |
|---|---|
| ZENNIUM PRO | Max current: ±3 A Max voltage: ±5 V / ±15 V 12 current ranges for the optimum current accuracy |
| PP212 | Power potentiostat for controlling the light intensity |
| TLS Wavelength range | 365 nm - 1020 nm |
IPCE-UV System
| Parameter | Value |
|---|---|
| ZENNIUM PRO | Max current: ±3 A Max voltage: ±5 V / ±15 V 12 current ranges for the optimum current accuracy |
| PP212 | Power potentiostat for controlling the light intensity |
| TLS wavelength range | 290 nm - 1020 nm |
Tunable Light Source
The TLS contains up to 25 or 29 LEDs depending upon the TLS type (without or with UV extension). The TLS also contains a white background light which may be used for the solar cells or photoelectrode with high light intensity threshold for photocurrents. The effect of the constant white background light is eliminated from the IPCE results.

Light Sources
Zahner offers a wide variety of light sources to choose from.
1) monochromatic LEDs (different LEDs available over a wide wavelength range).
2) tuneable light source (LED-based light source with wavelength range 295 - 1020 nm)
Accessories
Photoelectrochemical measurements are carried out in a controlled light environment. For this purpose, Zahner designed a light exclusion box (LEB). This LEB can accommodate the PECC cells and the TLS. The LEB also works as a Faraday cage and diminishes artefacts for low current measurements.

Light Exclusion Box
The Light Exclusion Box (LEB) is recommended for every photoelectrochemical / photovoltaic experiment. The LEB also works as a Faraday cage and eliminates the typical artifacts induced during low current measurements.

PEC-Cells
Photoelectrochemical cells (PECC) are designed for measurements of photoelectrodes. PEC cells are available with a window on electrolyte side (PECC-1) or with windows on electrolyte and working electrode side (PECC-2).
The PECC-2 allows front or back side illumination.